*Based on drop tests of lithium aluminosilicate versus single-tempered aluminosilicate glass, using rough sandpaper. 80% of samples survived a drop height 2x higher than conventional single-tempered aluminosilicate glass.
**Based on third party lab results conducted under the JIS Z 2801-2010 test standard. Contains a biocidalproduct: Dimethyloctadecyl[3-(trimethoxysilyl)propyl]ammonium chloride
†Rated 9H against low-carbon steel at 5H, using the ASTM D3363 Film Hardness by Pencil Test Hardness